ABSTRACT:
Taught is a method of sizing polyester yarn for weaving comprising the steps of applying thereto a latex having an acid pH and of a free radical initiated vinyl polymer having a weight average molecular weight of from about 300,000 to about 2,500,000, said polymer in dried film form being hydrophobic and not redispersible in a solution at a pH of from about 2 to 7 but redispersible by an aqueous alkaline medium, said polymer being prepared from monomers consisting essentially of by weight, 45-65% butyl acrylate a total of 28-45% styrene and/or methyl methacrylate and a total of 8-14% acrylic acid and/or methacrylic acid, and drying the yarn.
REFERENCES:
patent: 2807865 (1957-10-01), Shipee
patent: 3676207 (1972-07-01), Lofton et al.
patent: 4015317 (1977-04-01), Johnsen
patent: 4033922 (1977-07-01), Baron et al.
patent: 4106900 (1978-08-01), Perkins
patent: 4239671 (1980-12-01), Fink et al.
patent: 4248755 (1981-02-01), Williams
patent: 4312914 (1982-01-01), Guth
Fein Michael B.
Greenwald Harold L.
Lusignan Michael R.
Rohm and Haas Company
LandOfFree
Method of sizing polyester yarn does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of sizing polyester yarn, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of sizing polyester yarn will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-749368