Method of separating admixed contaminants from superalloy...

Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C148S674000, C210S222000, C210S758000, C210S774000

Reexamination Certificate

active

07153377

ABSTRACT:
A method is provided for separating superalloy metal powder from contaminants, such as process-produced contaminants, by enhancing the magnetic properties thereof in a carburizing atmosphere followed by magnetic separation of the contaminants from the superalloy metal powder to thereby enhance the concentration of the contaminants. Heating or mechanical agitation or both are employed to resist agglomeration of the metal powder before magnetic separation thereof from the contaminants. Certain preferred times and temperatures are disclosed.

REFERENCES:
patent: 1811032 (1931-06-01), Smith et al.
patent: 3516612 (1970-06-01), Fullman et al.
patent: 3544309 (1970-12-01), Fletcher et al.
patent: 3607236 (1971-09-01), Brooks et al.
patent: 3926789 (1975-12-01), Shubert
patent: 3953252 (1976-04-01), Levin et al.
patent: 3960617 (1976-06-01), Levin et al.
patent: 4054513 (1977-10-01), Windle
patent: RE30360 (1980-08-01), Shubert
patent: 4230750 (1980-10-01), Yurasko, Jr.
patent: 4259296 (1981-03-01), Hennion et al.
patent: 4312684 (1982-01-01), Chraplyvy et al.
patent: 4318735 (1982-03-01), Mishima et al.
patent: 4318757 (1982-03-01), Horimoto et al.
patent: 4347086 (1982-08-01), Chraplyvy et al.
patent: 4377410 (1983-03-01), Thomas et al.
patent: 4608093 (1986-08-01), Umemura et al.
patent: 4909865 (1990-03-01), Nakagawa et al.
patent: 5062904 (1991-11-01), Yoden
patent: 5749939 (1998-05-01), Kundrat
patent: 6447571 (2002-09-01), Ito et al.
patent: 2002/0144753 (2002-10-01), Yoshimura et al.
U.S. Appl. No. 10/420,126, filed Apr. 22, 2003, Spangler et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of separating admixed contaminants from superalloy... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of separating admixed contaminants from superalloy..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of separating admixed contaminants from superalloy... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3700061

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.