ABSTRACT:
This is a method for producing a composite grain structure in nickel-base superalloy articles by causing a controlled amount of grain growth in selected regions. The method uses alloys containing 0.01-1.0 carbon and 0.02-0.08 boron and a heat treatment in a non-reducing atmosphere after the alloy has been formed. The heat treatment causes diffusion of boron (but not carbon) in selected regions, lowering the amount of boron and causing controlled grain growth in these regions.

REFERENCES:
patent: 3741821 (1973-06-01), Athey et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of selective grain growth in nickel-base superalloys by c does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of selective grain growth in nickel-base superalloys by c, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of selective grain growth in nickel-base superalloys by c will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-904614

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.