Method of repairing damages in superalloys

Metal fusion bonding – Process – Repairing – restoring – or renewing product for reuse

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

228198, 228248, 419 9, 419 46, G23K 3102

Patent

active

050407180

ABSTRACT:
A method of repairing damages in a superalloy component is disclosed wherein existing brazed joints and protective coatings are not harmed. The method entails the use of a silicon-free metal mixture comprising (i) a low melting alloy having a liquidus below the temperature to be used to deposit the metal mixture, (ii) an alloy melting above about 2100.degree. F., and (iii) optionally nickel. The resultant repair has a solidus temperature of at least 1950.degree. F., preferably at least 2000.degree..

REFERENCES:
patent: 3155491 (1964-11-01), Hoppin
patent: 3246981 (1966-04-01), Quaas
patent: 3441409 (1969-04-01), Burr
patent: 3496630 (1970-02-01), Duff
patent: 3619182 (1971-11-01), Bieber et al.
patent: 3678570 (1972-07-01), Paulonis
patent: 3716347 (1973-02-01), Bergstrom et al.
patent: 3807993 (1974-04-01), Dalal et al.
patent: 4008844 (1977-02-01), Duvall
patent: 4219592 (1980-08-01), Anderson
patent: 4283225 (1981-08-01), Sexton
patent: 4285459 (1981-08-01), Baladjanian
patent: 4289833 (1981-09-01), Hachisuka
patent: 4444353 (1984-04-01), McMurray
patent: 4478638 (1984-10-01), Smith et al.
patent: 4556532 (1984-12-01), Umeha et al.
patent: 4614296 (1986-09-01), Lesgourgues

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of repairing damages in superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of repairing damages in superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of repairing damages in superalloys will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1002739

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.