Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal
Patent
1996-01-30
1998-04-21
Simmons, David A.
Metal treatment
Process of modifying or maintaining internal physical...
Heating or cooling of solid metal
148512, 148522, 148527, C22C 1907
Patent
active
057413789
ABSTRACT:
An improved method is described for restoring the mechanical properties to carbide-containing Co-based superalloy gas turbine components which have been exposed to high temperatures and pressures for extended periods of time. The method includes solution heat treating to 2250.degree.-2300.degree. F. for one to twelve hours to dissolve complex carbides, and aging at approximately 1965.degree.-1975.degree. F. for two to twenty four hours. The rejuvenated components exhibit excellent high temperature creep properties.
REFERENCES:
patent: 3667939 (1972-06-01), Hecht et al.
patent: 3802934 (1974-04-01), Augustine, Jr. et al.
patent: 3985582 (1976-10-01), Bibring et al.
patent: 4003765 (1977-01-01), Davidson
patent: 4008844 (1977-02-01), Duvall et al.
patent: 4078922 (1978-03-01), Magyar et al.
patent: 4116724 (1978-09-01), Hirschfeld et al.
patent: 4152181 (1979-05-01), Hirakis
patent: 4285459 (1981-08-01), Baladjanian et al.
patent: 4381944 (1983-05-01), Smith, Jr. et al.
patent: 4437913 (1984-03-01), Fukui et al.
patent: 4668265 (1987-05-01), Gaul et al.
patent: 4726101 (1988-02-01), Draghi et al.
patent: 4789412 (1988-12-01), Nakamura et al.
patent: 4830934 (1989-05-01), Ferrigno et al.
patent: 4938805 (1990-07-01), Haydon et al.
patent: 5086968 (1992-02-01), Fawley et al.
patent: 5156321 (1992-10-01), Liburdi et al.
patent: 5437737 (1995-08-01), Draghi et al.
Kurpaska S. Michael
Pietruska Norman
Phipps Margery S.
Simmons David A.
United Technologies Corporation
LandOfFree
Method of rejuvenating cobalt-base superalloy articles does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of rejuvenating cobalt-base superalloy articles, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of rejuvenating cobalt-base superalloy articles will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2054646