Method of reducing the gaping values in the web saw cut test on

Metal treatment – Process of modifying or maintaining internal physical... – Heating or cooling of solid metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148639, C21D 904

Patent

active

059163879

ABSTRACT:
This invention concerns a method of reducing the gaping values of railway tracks made of steel to less than 3.6 mm. It is characteristic of this invention that the rolled and leveled rails are heated briefly, i.e., for approx. 10 to 25 sec, until reaching a maximum temperature of 100.degree. C. in the rail head and a maximum of 260.degree. C. in the web, and then they are allowed to cool again immediately.

REFERENCES:
patent: 3525326 (1970-08-01), Deal

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of reducing the gaping values in the web saw cut test on does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of reducing the gaping values in the web saw cut test on , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing the gaping values in the web saw cut test on will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1372693

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.