ABSTRACT:
Iron ore particles are partially reduced by passing through a rotary kiln countercurrent to flowing hydrogen and carbon monoxide. The partially reduced ore is then fed into a plasma arc torch wherein the reduction is completed. The off-gas from the arc torch is reacted with methane to reform the water vapor in the off-gas into hydrogen and carbon monoxide which are used to partially reduce the iron ore particles in the rotary kiln.

REFERENCES:
patent: 2805930 (1957-09-01), Udy
patent: 2894831 (1959-07-01), Old
patent: 3140168 (1964-07-01), Halley
patent: 3163520 (1964-12-01), Collin
patent: 3163521 (1964-12-01), Rinesch
patent: 3475160 (1969-10-01), Heinzelmann
patent: 3761244 (1973-09-01), Hoffert
patent: 3770421 (1973-11-01), Celada

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of reducing iron oxide does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of reducing iron oxide, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing iron oxide will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-229363

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.