ABSTRACT:
Pelletized iron ore is introduced into a shaft furnace and reduced in a countercurrent stream of reducing gas at a hot zone temperature of 1375.degree.F to 1700.degree.F. The pellets have a low silica content and, prior to indurating, a high moisture content, providing a highly porous texture which results in improved reducibility.

REFERENCES:
patent: 2511400 (1950-06-01), de Jahn
patent: 3682621 (1972-08-01), Struve et al.
patent: 3759693 (1973-08-01), Kunii et al.
Ball et al., Agglomeration of Iron Ores, p. 256, Am. Elsevier Pub. Co., Apr. 4, 1974.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of reducing iron ore does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of reducing iron ore, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing iron ore will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2233114

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.