ABSTRACT:
A method of making glasses with manufacturing systems employing platinum or molybdenum melting, fining delivery, or forming vessel, wherein the partial pressure of hydrogen outside the vessel is controlled or manipulated, relative to the partial pressure of hydrogen inside the platinum structure, to minimize surface blistering in the glass in contact with the platinum or molybdenum.
REFERENCES:
patent: 2009764 (1935-07-01), Dalton
patent: 2982053 (1961-11-01), Elmer
patent: 3233993 (1966-02-01), Weidel
patent: 3338696 (1967-08-01), Dockerty
patent: 3682609 (1972-08-01), Dockerty
patent: 3850602 (1974-11-01), Bruning
patent: 3954656 (1976-05-01), Deeg et al.
patent: 4704153 (1987-11-01), Schwenninger et al.
patent: 4738938 (1988-04-01), Kunkle et al.
patent: 4983198 (1991-01-01), Ogino
patent: 5509951 (1996-04-01), Baucke et al.
patent: 5688300 (1997-11-01), Ashley et al.
Ebba de kever and Gunther Heinz Frischat, "Influence of batch moisture and atmosphere on the melting behavior of As.sub.2 O.sub.3 -and Sb.sub.2 O.sub.3 -containing glasses", Glastechnische Berichte, Feb. 1992, pp. 64-66.
Edith M. Firth, F.W. Hodkin, Michael Parkin, W.E.S. Turner, "The Effect of Moisture on the Melting, Working, and other Properties of Totash-Lead Oxide-Silica Glasses of the `English Crystal` Type", Journal of the Society of Glass Technology, 1926. vol. X., pp. 220-229.
S.M. Budd, V.H. Exelby and J.J. Kirwan, "The Formation of Gas Bubbles in Glass at High Temperature", Glass Technology vol. 3 No. 4 Aug. 1962, pp. 124-129.
M. Boffe, G. Percriaux and E. Plumat, "Formation of Bubbles During Devitrification and Remelting of Crystals in Glass", Nucleation and Crystallization Symposium, pp. 47-54.
J.E. Fenstermacher, R.C. Lesser and R.J. Ryder, "A Study of Water Content of Container Glasses", The Glass Industry/Sep. 1965, pp. 518-521.
Dr. J.P. Poole, "Fundamentals of Fining", Commission on Glass, Annual Meeting, Toronto, Canada, 1969. pp. 169-176.
Dr. Horst Scholze, "Gases and Water in Glass", Part one, Lectures on Glass and Technology, Rensselaer Polytechnic Institute, Troy, NY, Mar. 30-Apr. 1, 1996. 19 pages.
Robert J. Eagan and Gary J. Jones, "Bubble Formation in Glass by Reaction with Silicon and Silicon-Germanium Alloys", Sep. 2, 1992. pp. 300-301.
Dorfeld William G.
Lineman David M.
Carlson Robert L.
Chin Peter
Corning Incorporated
Ruller Jacqueline A.
LandOfFree
Method of reducing bubbles at the vessel/glass interface in a gl does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of reducing bubbles at the vessel/glass interface in a gl, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of reducing bubbles at the vessel/glass interface in a gl will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-19378