ABSTRACT:
A method of recycling commingled plastics waste containing min. 30 wt. % of polyolefins to a tough thermoplastic material, based on the compatibilization of the polymer components of commingled plastics waste with an admixture of 2-15 wt. % of an ethylene--propylene copolymer or a styrene--butadiene block copolymer or a combination of an ethylene--propylene copolymer and a styrene--butadiene copolymer in any weight ratio, together with 0.1-2.5 wt. % of a secondary aromatic amine and by subsequent blend processing in the melt.

REFERENCES:
patent: 4212789 (1980-07-01), Anspon
patent: 6784233 (2004-08-01), Weber et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of recycling of commingled plastics waste to tough... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of recycling of commingled plastics waste to tough..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of recycling of commingled plastics waste to tough... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4090377

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.