ABSTRACT:
Scrap foam of flexible or semi-rigid polyurethane is pyrolized at 450.degree.-800.degree. C., preferably 600.degree. C., in the absence of air and of any added reactive agents or catalysts. The residence time may be from 3 minutes to one hour, preferably about 5 minutes. A distillate is obtained comprising an aqueous phase and an organic phase. The latter essentially consists of alcohols and polyols and may be re-used as such for preparing polyurethane resins.

REFERENCES:
patent: 2998395 (1961-08-01), Albert et al.
patent: 3983087 (1976-09-01), Tucker et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of recovering polyols from scrap polyurethane foam does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of recovering polyols from scrap polyurethane foam, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of recovering polyols from scrap polyurethane foam will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-284155

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.