Method of production of a reinforced optical fiber

Coating processes – Optical element produced – Polarizer – windshield – optical fiber – projection screen – or...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

350 9623, 350 9634, 4273897, 4274072, G02B 644, B05D 506

Patent

active

047254530

ABSTRACT:
A reinforced optical fiber includes a reinforcing inner layer interposed between a buffer layer of silicon rubber and a FRP layer made of styrene resin and fibers. The reinforcing inner layer is formed by binding filaments attached longitudinally onto the buffer layer with a non-styrene resin. The additional reinforcing inner layer improves crushing resistance and also keeps low an increase of transmission loss. The reinforcing inner layer directly covering the buffer layer is formed by the steps of longitudinally attaching dry filaments to the buffer layer and then impregnating the filaments with a curable resin.

REFERENCES:
patent: 4113349 (1978-09-01), Stiles
patent: 4505541 (1985-03-01), Considine et al.
patent: 4629286 (1986-12-01), Fuse et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of production of a reinforced optical fiber does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of production of a reinforced optical fiber, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of production of a reinforced optical fiber will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2220277

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.