ABSTRACT:
Weakly acidic cationic ion exchange resin particles are charged with uranyl ions by contacting the particles step wise with aqueous uranyl nitrate solution at higher uranium concentrations from stage to stage. An alkaline medium is added to the uranyl nitrate solution in each stage to increase the successive pH values of the uranyl nitrate solution contacting the particles in dependence upon the uranium concentration effective for maximum charging of the particles with uranyl ions.

REFERENCES:
patent: 3438749 (1969-04-01), Lonadier
patent: 3800023 (1974-03-01), Haas
patent: 3995009 (1976-11-01), Notz
patent: 4070438 (1978-01-01), Notz et al.
Haas, "HTGR Fuel Development: Loading of Uranium on Carboxylic Acid Catioxchange Resins Using Solvent Extraction of Nitrate", ORNL-TM-4955, pp. 1-12, (9-1975).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing weakly acidic cation exchange resin particle does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing weakly acidic cation exchange resin particle, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing weakly acidic cation exchange resin particle will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2433039

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.