Method of producing thin-walled castings

Metal founding – Process – Shaping liquid metal against a forming surface

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

164122, 75123CB, B22D 1502, B22D 2704

Patent

active

040570983

ABSTRACT:
A method of producing castings comprising the steps of: pouring moulds with inoculated cast iron containing, by weight per cent: carbon 3.6-3.8, silicon 2.8-3.2, manganese up to 0.4, magnesium not more than 0.01, at a melt temperature ranging from 1420.degree. to 1450.degree. C, and subsequently cooling the cast iron. The thickness of walls of the castings is chosen so that the initial cooling rate is 10.degree.-14.degree. C/sec with a preset heat conductivity.

REFERENCES:
patent: 3726670 (1973-04-01), Kusoka
P. R. Beeley, Foundry Technology, Holsted Press Division, John Wiley & Sons, Inc., New York, 1972, p. 330.
"Production of Ductile Iron Castings", by J. W. Curry, pp. 373-375 in ASM Metals Handbook, 8th Edition, vol. 5, Forging & Casting, 1970.
Gray and Ductile Iron Castings Handbook, 1971, Chapter 3, "Metallurgy of Cast Iron", pp. 93-127.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing thin-walled castings does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing thin-walled castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing thin-walled castings will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-225504

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.