ABSTRACT:
A method of producing steel plate having a low yield ratio and high strength and a dual-phase mixed microstructure of ferrite and second-phase carbide comprises heating to at least 950.degree. C. low-carbon slab steel having 0.30% or less carbon, 0.05 to 0.60% silicon, 0.5 to 2.5% manganese, and 0.01 to 0.10% aluminum as the basic components, with the balance being iron and unavoidable impurities, or low-carbon low-alloy slab steel comprising in addition to the above basic components one or more elements selected from copper, nickel, chromium, molybdenum, niobium, vanadium, titanium, boron and calcium, hot rolling it, reheating it and tempering it.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing steel having a low yield ratio does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing steel having a low yield ratio, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing steel having a low yield ratio will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1884370

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.