ABSTRACT:
A method for producing a silicon nitride honeycomb filter, which comprises heat-treating in a nitrogen atmosphere a green body comprising from 50 to 85 mass % of metal silicon particles having an average particle diameter of from 5 to 50 μm, from 5 to 30 mass % of glass hollow particles having a softening temperature of from 400 to 1000° C. and from 10 to 20 mass % of an organic binder to convert metal silicon substantially to silicon nitride.

REFERENCES:
patent: 5004709 (1991-04-01), Stranford et al.
patent: 5756411 (1998-05-01), Nakahata et al.
patent: 6565797 (2003-05-01), Miyakawa et al.
patent: 6593261 (2003-07-01), Shinohara et al.
patent: 6849213 (2005-02-01), Miyakawa et al.
patent: 2003/0006518 (2003-01-01), Miyakawa et al.
patent: 2003/0186801 (2003-10-01), Inoue et al.
patent: 2005/0023735 (2005-02-01), Miyakawa et al.
patent: 2005/0023736 (2005-02-01), Matsuzaki et al.
patent: 2005/0043166 (2005-02-01), Shinohara et al.
patent: 784038 (1997-07-01), None
patent: 1 160 223 (2001-12-01), None
patent: 1 167 321 (2002-01-01), None
patent: 52-121613 (1977-10-01), None
patent: 6-256069 (1994-09-01), None
patent: 7-187845 (1995-07-01), None
patent: 8-59364 (1996-03-01), None
patent: 2002-284585 (2002-10-01), None
patent: WO 8800933 (1988-02-01), None
patent: WO 01/47833 (2001-07-01), None
patent: WO 2004/050318 (2004-06-01), None
patent: WO 2004/067147 (2004-08-01), None
U.S. Appl. No. 10/901,171, filed Jul. 29, 2004, Shinohara, et al.
U.S. Appl. No. 10/892,200, filed Jul. 16, 2004, Miyakawa et al.
U.S. Appl. No. 10/216,815, filed Aug. 13, 2002, Miyakawa et al.
U.S. Appl. No. 09/975,262, filed Oct. 12, 2001, Miyakawa.
U.S. Appl. No. 10/140,162, filed May 8, 2002, Miyakawa.
U.S. Appl. No. 10/900,090, filed Jul. 28, 2004, Matsuzaki et al.
U.S. Appl. No. 10/901,158, filed Jul. 29, 2004, Suzuki et al.
U.S. Appl. No. 11/240,509, filed Oct. 3, 2005, Shinohara et al.
U.S. Appl. No. 11/287,461, filed Nov. 28, 2005, Shinohara et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing silicon nitride honeycomb filter does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing silicon nitride honeycomb filter, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing silicon nitride honeycomb filter will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3658312

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.