ABSTRACT:
A method of producing primarily tempered martensite steel comprising the steps of cutting low carbon--high manganese steel into usable size pieces, shaping the pieces without surface fraction of the pieces, heating the pieces to approximately 1650.degree. F. and quenching the pieces in water before the pieces cool below approximately 1475.degree. F.

REFERENCES:
patent: 3944442 (1976-03-01), Donachie

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing primarily tempered martensite steel does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing primarily tempered martensite steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing primarily tempered martensite steel will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1988762

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.