Single-crystal – oriented-crystal – and epitaxy growth processes; – Forming from vapor or gaseous state – With a step of measuring – testing – or sensing
Reexamination Certificate
2008-01-29
2008-01-29
Hiteshew, Felisa (Department: 1722)
Single-crystal, oriented-crystal, and epitaxy growth processes;
Forming from vapor or gaseous state
With a step of measuring, testing, or sensing
C117S951000, C117S952000, C423S062000
Reexamination Certificate
active
07323050
ABSTRACT:
A method of producing a lithium-tantalate crystal, wherein at least a first material containing lithium tantalate, lithium niobate or hydrogen storage alloy storing hydrogen that is subjected to a heat treatment at a temperature of T1′ that is Curie temperature or higher in a reducing atmosphere is superposed on a single-polarized lithium-tantalate crystal, and then the crystal is subjected to a heat treatment at a temperature of T2′ that is lower than Curie temperature in a reducing atmosphere, thereby an electric conductivity of the single-polarized lithium-tantalate crystal is increased. There can be provided a method of producing a lithium-tantalate crystal wherein the surface charge generated by applying a temperature change to the lithium-tantalate crystal can be decayed quickly without accumulating by increasing the electric conductivity, and an effective piezoelectric property is exhibited by maintaining the single polarized structure.
REFERENCES:
patent: 4371419 (1983-02-01), Fukuda et al.
patent: 5323262 (1994-06-01), Mizuuchi et al.
patent: 5910699 (1999-06-01), Namba et al.
patent: 6319430 (2001-11-01), Bordui et al.
patent: 6348094 (2002-02-01), Shiono et al.
patent: 2005/0066879 (2005-03-01), Shiono
patent: 0 893 515 (1999-01-01), None
patent: 1 043 617 (2000-10-01), None
patent: A 53-109900 (1978-09-01), None
patent: A 54-12587 (1979-01-01), None
patent: A 57-3800 (1982-01-01), None
patent: A 58-151399 (1983-09-01), None
patent: A 10-1391 (1998-01-01), None
patent: A 11-92147 (1999-04-01), None
patent: WO 01/33260 (2001-05-01), None
patent: WO 2004/002891 (2004-01-01), None
Hiteshew Felisa
Oliff & Berridg,e PLC
Shin-Etsu Chemical Co. , Ltd.
LandOfFree
Method of producing lithium tantalate crystal does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of producing lithium tantalate crystal, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing lithium tantalate crystal will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2794239