ABSTRACT:
An ethylene-vinylalcohol copolymer film is prepared by biaxially or multiaxially stretching a nonstretched ethylene-vinylalcohol polymer film having a moisture content of not more than 3.5%, said ethylenevinyl alcohol copolymer having an ethylene content of 20 to 55 mole % and a saponification degree of not less than 96 mole % and said stretching being conducted within a temperature range of 50.degree. to 150.degree. C. to such an extent that the film is expanded to an area 4 to 20 times the original area.

REFERENCES:
patent: 3419654 (1968-12-01), Chiba et al.
patent: 3440316 (1969-04-01), Miyake et al.
patent: 3585177 (1971-06-01), Gardner et al.
patent: 3595740 (1971-07-01), Geson

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing ethylene-vinyl alcohol copolymer film does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing ethylene-vinyl alcohol copolymer film, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing ethylene-vinyl alcohol copolymer film will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-931783

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.