ABSTRACT:
A copper-iron-aluminum hydrogenation catalyst is prepared by separately and simultaneously adding dropwise to a bath of water (a) an aqueous solution of cupric, ferrous and aluminum salts and (b) an aqueous solution of alkali metal compound effective to precipitate the copper, iron and aluminum ions, and then agitating the reaction mixture at a temperature of at least 50.degree. C., at a pH of 9.5 to 11.5, for from 10 minutes to 10 hours, then recovering the precipitate and treating it to convert it to an active catalyst.

REFERENCES:
patent: 2449295 (1948-09-01), Gutzeit
patent: 2844633 (1958-07-01), Braconier et al.
patent: 3197418 (1965-07-01), Maebashi et al.
patent: 4144198 (1979-03-01), Miya et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing copper-iron-aluminum catalysts does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing copper-iron-aluminum catalysts, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing copper-iron-aluminum catalysts will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1408470

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.