ABSTRACT:
Copper-clad steel wire is produced by forming a copper tube around the wire, and drawing down the copper tube and wire to reduce the cross-section of the wire by at least 30%. The wire is annealed, slowly cooled and the cross-section further reduced by at least 10%.

REFERENCES:
patent: RE28526 (1975-08-01), Ziemek
patent: 2063470 (1936-12-01), Staples
patent: 3463620 (1969-08-01), Winter
patent: 3894675 (1975-07-01), Klebl et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing copper clad steel wire does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing copper clad steel wire, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing copper clad steel wire will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-648191

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.