ABSTRACT:
A processing sequence is described for producing specific controlled elongated oriented crystal structures in nickel base superalloys. The method is performed in the solid state. Superalloy material is provided in a dense workable form. The material is cold straight rolled and cold cross rolled with intermediate anneals. This sequence produces a particular texture or preferred orientation in the rolled article. This textured article is then directionally recrystallized to produce the desired final microstructure comprised of aligned elongated grains of a particular controllable orientation.

REFERENCES:
patent: 3346427 (1967-10-01), Baldwin, Jr. et al.
patent: 3787205 (1974-01-01), Church
patent: 3902900 (1975-09-01), Restall
patent: 3920489 (1975-11-01), Buchanan
patent: 3982973 (1976-09-01), Peters et al.
patent: 3992161 (1976-11-01), Cairns et al.
patent: 4002503 (1977-01-01), Bourne et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing columnar crystal superalloy material with co does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing columnar crystal superalloy material with co, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing columnar crystal superalloy material with co will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1536575

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.