ABSTRACT:
A method for processing CoPt alloys with improved magnetic properties. The method includes sealing a sample of a CoPt alloy in an evacuated quartz tube, and heating the alloy to a temperature of approximately 1000 degrees C. to homogenize the alloy for approximately 3 hours. The sample is then cooled at a controlled cooling rate of 120-150 degrees C. per minute to 600 degrees C. The sample is then held at 600 degrees C. for 10 hours to promote isothermal ordering. Finally, the sample is quenched in mineral oil.

REFERENCES:
patent: 2622050 (1952-12-01), Martin et al.
patent: 4983230 (1991-01-01), Overfelt et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing cobalt-platinum magnetic alloys with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing cobalt-platinum magnetic alloys with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing cobalt-platinum magnetic alloys with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-4219946

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.