Method of producing and joining superalloy balls by means of...

Stock material or miscellaneous articles – All metal or with adjacent metals – Composite powder

Reexamination Certificate

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C428S613000, C075S246000, C419S002000, C419S023000, C419S036000

Reexamination Certificate

active

07968207

ABSTRACT:
The invention relates to a method of producing and joining superalloy balls by means of brazing and to objects produced with such joints. According to one aspect of the invention, an alloy powder covered with a brazing solder is bonded to a spherical core and subsequently transformed into a continuous alloy layer by means of brazing.

REFERENCES:
patent: 3135044 (1964-06-01), Mote, Jr. et al.
patent: 3383207 (1968-05-01), Butts
patent: 3508599 (1970-04-01), Vordahl
patent: 3781170 (1973-12-01), Nakao et al.
patent: 4013461 (1977-03-01), Elbert
patent: 4043381 (1977-08-01), Mazdiyasni et al.
patent: 4775598 (1988-10-01), Jaeckel
patent: 5073459 (1991-12-01), Smarsly et al.
patent: 6463759 (2002-10-01), Garcia et al.
patent: 6887519 (2005-05-01), Pillhoffer et al.
patent: 7544322 (2009-06-01), Nadler et al.
patent: 1 490 744 (1967-08-01), None
patent: 2 094 258 (1972-02-01), None
patent: 2 278 794 (1976-02-01), None
patent: 2585445 (1987-01-01), None
patent: 2 638 174 (1990-04-01), None
patent: 2 777 215 (1999-10-01), None
patent: 2 853 329 (2004-10-01), None
patent: 59-220350 (1984-12-01), None
patent: 2-256579 (1990-10-01), None
Machine translation of FR 2777215. Oct. 1999.
International Search Report, dated Feb. 6, 2007, corresponding to PCT/FR2006/001643.
Queheillalt, et al., “Ultrasonic characterization of cellular metal structures,” Apr. 19, 2006, p. 1, Database Compendez (Online) Engineering Information, Inc., N.Y., N.Y., U.S., XP002376854, Database accession No. E2002096870581, abrégé, abstract only.
Queheillalt, et al., “Ultrasonic characterization of cellular metal structures,” Material Science and Engineering A323 (2002) pp. 138-147, XP-002376786.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing and joining superalloy balls by means of... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing and joining superalloy balls by means of..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing and joining superalloy balls by means of... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2656520

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.