ABSTRACT:
A method of producing a nickel electrode comprising a current collector and active material pressed into physical and electrical contact with the current collector. The active material comprises nickel hydroxide, an organic binder, a conductive diluent and a cobalt compound, the cobalt compound having been precipitated from a cobalt-containing solution in contact with the already-formed nickel hydroxide.
REFERENCES:
patent: 3066178 (1962-11-01), Winkler
patent: 3108910 (1963-10-01), Herold
patent: 3657013 (1972-04-01), Melin
patent: 3725129 (1973-04-01), Ruzzo, Jr.
patent: 3752706 (1973-08-01), Melin
patent: 3928068 (1975-12-01), Jackovitz et al.
patent: 4029132 (1977-06-01), Jackovitz et al.
patent: 4049027 (1977-09-01), Seiger
patent: 4063576 (1977-12-01), Gunther
patent: 4130696 (1978-12-01), Gunther
Iwaki, et al., "Nickel Electrode for an Alkaline Battery," Chem. Abs., 88:155729k, p. 189 (May 29, 1978).
Yamazaki, et al., "Nickel Electrode for Alkaline Storage Battery" Chem. Abs., 89:8914; p. 158 (Jul. 10, 1978).
Kuzmin, Yu, et al., Chem. Abs., 80:9712t, p. 455 (Jan. 14, 1974).
Brown David J.
Reid Michael
Crane Daniel C.
Lucas Industries Limited
LandOfFree
Method of producing a nickel electrode does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of producing a nickel electrode, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing a nickel electrode will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-402236