Method of preventing stress corrosion in a bellows expansion joi

Cleaning and liquid contact with solids – Processes – Hollow work – internal surface treatment

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

134 27, 285 41, 285 47, 285 48, 285 50, 285 55, 285226, 285227, 252387, 252390, B08B 900, B08B 3000, F16L 5300, F16L 1112

Patent

active

046683038

ABSTRACT:
A novel bellows expansion joint design and method of preventing stress corrosion cracking incorporates an internal cylindrical weir or sleeve which defines an inner flushing chamber adjacent the expansion bellows wherein connections are provided on the exterior wall of the expansion joint body to allow the admission of a chemical solution or treating fluid directly onto the inside surface of the bellows from an external connection to the expansion joint. In addition, a further connection is provided to a second flushing chamber surrounding the exterior of the bellows so that a similar solution may be admitted and allowed to overflow from an upper portion of the chamber.

REFERENCES:
patent: 2291085 (1942-07-01), Lehmfouhl et al.
patent: 2520751 (1950-08-01), Zucrow
patent: 2536793 (1951-01-01), Andersson et al.
patent: 2651104 (1953-09-01), Ginos
patent: 2823150 (1958-02-01), Henricks
patent: 3067070 (1962-12-01), Loucks
patent: 3127200 (1964-03-01), Loyog
patent: 3186721 (1965-06-01), Petri
patent: 3232640 (1966-02-01), Donkle, Jr.
patent: 3488067 (1970-01-01), Sommer
patent: 3496017 (1970-02-01), Weed
patent: 3517949 (1970-06-01), Hirai et al.
patent: 3522093 (1970-07-01), Woolman
patent: 3536081 (1970-10-01), Riess
patent: 3811713 (1974-05-01), Barrett et al.
patent: 3874708 (1975-04-01), Gresenr
patent: 3901839 (1975-08-01), Jjerman
patent: 4045056 (1977-08-01), Kandokov et al.
patent: 4165107 (1979-08-01), Offo et al.
patent: 4308076 (1981-12-01), Knowlton
patent: 4317685 (1982-03-01), Ahuja et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of preventing stress corrosion in a bellows expansion joi does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preventing stress corrosion in a bellows expansion joi, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preventing stress corrosion in a bellows expansion joi will most certainly appreciate the feedback.