ABSTRACT:
Hydrogen peroxide or a hydrogen peroxide producing agent is added to a water system having copper or copper alloy such as a thermal storage water system or a closed water system whereby the concentration of hydrogen peroxide in the circulating water becomes 1 to 200 mgH.sub.2 O.sub.2 /L. Hydrogen peroxide produces oxygen and oxygen works microbes directly so as to remove the microbial fouling and thus prevent the pitting corrosion in copper or its alloy due to microbial contamination.
REFERENCES:
patent: 4806169 (1989-02-01), Spane et al.
Bhat Nina
Kurita Water Industries Ltd.
LandOfFree
Method of preventing pitting corrosion does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of preventing pitting corrosion, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preventing pitting corrosion will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-10045