ABSTRACT:
A method for extracting vanadium pentoxide from metallurgical slags containing vanadium with a ratio of (V.sub.2 O.sub.5 /CaO) being greater than 0.05 including roasting in an oxidizing medium a slag which has been disintegrated to a particle size less than 0.1 mm and then processing the roasted particles with solutions of phosphoric acid containing from 5 to 20 per cent by weight of H.sub.3 PO.sub.4, with a liquid-to-solid ratio of from 2-10:1 at a temperature of from 50.degree. - 100.degree. C for a period of time from 30 to 120 minutes.

REFERENCES:
patent: 2168169 (1939-08-01), Mayer
patent: 2183027 (1939-12-01), Mayer
patent: 2197241 (1940-04-01), Hatherell
patent: 2822240 (1958-02-01), Dunn et al.
patent: 3840637 (1974-10-01), Hendwick et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing vanadium pentoxide from metallurgical slags does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing vanadium pentoxide from metallurgical slags , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing vanadium pentoxide from metallurgical slags will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2299112

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.