ABSTRACT:
In an overbased sulfonate process calcium hydroxide is formed in situ by the continuous and uniform addition of water to calcium oxide over the entire hydration and carbonation time rather than incrementally. It has been found that the water rate and amount are critical.
A 300 TBN product is formed with an H.sub.2 O/CaO molar ratio of 0.4 and a 3 hour hydration time. A 400 TBN product is formed with an H.sub.2 O/CaO molar ratio of 0.8 and 3 hour hydration time.
Improved filterability and raw material utilization as well as reduced by-product solids content is achieved.

REFERENCES:
patent: 3830739 (1974-08-01), Kemp
patent: 4192758 (1980-03-01), Dickey et al.
patent: 4235810 (1980-11-01), Osselet et al.
patent: 4543194 (1985-09-01), Spence et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing overbased calcium sulfonates does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing overbased calcium sulfonates, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing overbased calcium sulfonates will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-967820

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.