ABSTRACT:
A loosely aggregated 200-500 millimicron primary particle size silica can be produced by a silicate neutralization technique. The process consists of neutralizing an alkali metal silicate solution by addition to an ammoniated acetic acid or carbonic acid mixture. These particles are loosely aggregated to an average particle size of about 1 micron. These particles are readily deaggregated in a fluid energy mill. A very convenient technique is to dry and deaggregate in a fluid energy mill in a single step.

REFERENCES:
patent: 2856268 (1958-10-01), Young
patent: 3165379 (1965-01-01), Schwartz
patent: 3208823 (1965-09-01), Baker et al.
patent: 3367742 (1968-02-01), Marotta et al.
patent: 3787561 (1974-01-01), Acker et al.
patent: 3798174 (1974-03-01), Acker et al.
patent: 3862104 (1975-01-01), Witt

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing loosely aggregated 200-500 millimicron silic does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing loosely aggregated 200-500 millimicron silic, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing loosely aggregated 200-500 millimicron silic will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-671570

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.