Synthetic resins or natural rubbers -- part of the class 520 ser – Synthetic resins – Polymers from only ethylenic monomers or processes of...
Patent
1976-04-09
1977-11-29
Lilling, Herbert J.
Synthetic resins or natural rubbers -- part of the class 520 ser
Synthetic resins
Polymers from only ethylenic monomers or processes of...
162168N, 162168NA, 428514, 526307, 526312, C08F 2070, C08F 2258, C08F22060, C08F22600
Patent
active
040606791
ABSTRACT:
A paper size comprising a water-soluble salt of a copolymer of from 30 to 85% by weight of olefins of 2 to 12 carbon atoms, having a terminal double bond, and/or vinyl ethers, and from 15 to 70% by weight of basic acrylic and/or methacrylic compounds, which copolymer has a molecular weight of from 600 to 4,500 and is manufactured by continuous copolymerization at from 130.degree. to 320.degree. C.
REFERENCES:
patent: 2595907 (1952-05-01), Thomas et al.
patent: 2654729 (1953-10-01), Price
patent: 2879255 (1959-03-01), Coover
patent: 2980657 (1961-04-01), Melamed
patent: 3040012 (1962-06-01), Maeder
patent: 3043822 (1962-07-01), Maeder
patent: 3186973 (1965-06-01), Maeder
patent: 3308081 (1967-03-01), Glabisch
patent: 3395198 (1968-07-01), Taniguchi et al.
patent: 3541037 (1970-11-01), Finn et al.
patent: 3629209 (1971-12-01), McDonald et al.
patent: 3873646 (1975-03-01), Hoke
Gausepohl Hermann
Naarmann Herbert
Reichel Fritz
BASF - Aktiengesellschaft
Lilling Herbert J.
LandOfFree
Method of preparing a low molecular weight paper size polymer by does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of preparing a low molecular weight paper size polymer by, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing a low molecular weight paper size polymer by will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1634146