ABSTRACT:
A sintered compact of cubic boron nitride is made by adsorbing and/or diffusing 0.005 to 1.000 percent by weight of water into a boron nitride compact containing alkaline earth metal boron nitride as a catalyst. The so prepared compact is then subjected to a treatment under high pressure at a relatively low temperature to form a dense cubic boron nitride sintered compact of high purity.
REFERENCES:
patent: 2947617 (1960-08-01), Wentorf
patent: 3212852 (1965-10-01), Bundy
patent: 4188194 (1980-02-01), Corrigan
patent: 4349517 (1982-09-01), Lysanov et al.
patent: 4469802 (1984-09-01), Endo et al.
Mat. Res. Bull., vol. 7, 999-1004, 1972, Pergamon Press, Inc., M. Waktsuki et al. "Synthesis of Polycrystalline Cubic Bn".
Mat. Res. Bull., vol. 9, pp. 1443-1446, 1974, Pergamon Press Inc., K. Susa et al. "Catalytic Effect of Water the Synthesis of Cubic BN".
Ota Nobuhiro
Sumiya Hitoshi
Yazu Shuji
Brunsman David M.
Capella Steven
Fasse W. G.
Kane, Jr. D. H.
Sumitomo Electric Industries Ltd.
LandOfFree
Method of manufacturing sintered compact of cubic boron nitride does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of manufacturing sintered compact of cubic boron nitride, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing sintered compact of cubic boron nitride will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-1748475