ABSTRACT:
A rolled steel product is given an elastic limit of 500 to 1200 MPa by selection of a particular steel composition and a particular heat treatment. The steel contains 0.10-0.50% C, 0.90-1.50% Mn, and 0.10-0.45% Si, and optionally 0.20-0.70% Ni, 0.10-0.80% Cr, and 0.02-0.10% V. The heat treatment consists of surface quenching from above the austenitization temperature by means of a fluid, the heat remaining in the product being sufficient to temper the martensite and/or bainite in the quenched surface.

REFERENCES:
patent: 3666572 (1972-05-01), Nakagawa et al.
patent: 4016009 (1977-04-01), Economopoulos
patent: 4016015 (1977-04-01), Respen et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing rolled steel products with high elastic does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing rolled steel products with high elastic , we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing rolled steel products with high elastic will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1489304

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.