ABSTRACT:
Halogenation of Udel (trademark) and Radel (trademark) polysulfone occurs adily by electrophilic substitution. The reactive substitution position is situated ortho- to the aryl ether linkage in the Bisphenol-A portion of the repeat units. Halogenated polysulfones are obtained by reaction of the polymer with elemental halogen. Thus, a solution of Udel polysulfone in chloroform, treated with excess bromine at room temperature, gives dibrominated polysulfone III in high yield. The degree of substitution after 18-24 hours is typically 1.80 to 2.05 by bromine analysis. Similar results are obtained by reaction of the polymer with elemental chlorine. Lower degrees of substitution are obtained with shorter reaction times or using lesser amounts of halogen.

REFERENCES:
patent: 4797457 (1989-01-01), Guiver et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing halogenated aromatic polysulfone compoun does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing halogenated aromatic polysulfone compoun, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing halogenated aromatic polysulfone compoun will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-294511

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.