Details

C428S457000, C428S624000, C428S675000, C205S125000, C205S239000, C205S291000, C134S003000, C216S108000, C427S309000, C427S435000

Reexamination Certificate

active

10483612

ABSTRACT:
The object is to provide a method of manufacturing electrodeposited copper foil with a carrier foil for high-temperature heat-resistance in which the peeling of the carrier foil is easy even by press working at temperatures of not less than 200°C. For this purpose are adopted “a method of manufacturing electrodeposited copper foil with a carrier foil for high-temperature heat-resistance in which an organic adhesive interface layer is formed on a surface of carrier foil by use of an organic agent, and an electrodeposited copper foil layer is formed on the organic adhesive interface layer, characterized in that the formation of the organic adhesive interface layer on the surface of the carrier foil is performed by acid pickling the surface of the carrier foil by use of an acid pickling solution containing 50 ppm to 2000 ppm of organic agent used in the formation of the adhesive interface layer and by simultaneously causing the organic agent to be adsorbed whereby an acid pickled and adsorbed organic film is formed” and others.

REFERENCES:
patent: 6319620 (2001-11-01), Kataoka et al.
patent: 6610418 (2003-08-01), Yoshioka et al.
patent: 6777108 (2004-08-01), Obata et al.
patent: 2003/0148136 (2003-08-01), Yamamoto et al.
patent: 2004/0067377 (2004-04-01), Sugimoto et al.
patent: 960725 (1999-12-01), None
patent: 996318 (2000-04-01), None
patent: 2000-151068 (2000-05-01), None
patent: 2000-309898 (2000-11-01), None
patent: 2001-140091 (2001-05-01), None
patent: WO 98/51485 (1998-11-01), None

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing electrodeposited copper foil with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing electrodeposited copper foil with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing electrodeposited copper foil with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3809141

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.