Method of manufacturing a hollow silicon carbide fiber reinforce

Coating processes – Coating by vapor – gas – or smoke – Carbon or carbide coating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264 81, 427226, 427227, 427294, 4274197, C23C 1600, B05D 302

Patent

active

053824539

ABSTRACT:
Carbon coated carbide fibers are arranged in a predetermined pattern and shape around a silicon carbide coated graphite insert. Silicon carbide is infiltrated into the silicon carbide fibers to produce a SiC/SiC composite component. The SiC/SiC composite component is coated with glass and is then heated in air to burn out the graphite insert to form a hollow glass coated SiC/SiC composite component. The method is suitable for producing hollow SiC/SiC composite turbine blades or vanes.

REFERENCES:
patent: 3961003 (1976-06-01), Parsels
patent: 4980202 (1990-12-01), Brennan et al.
patent: 5018271 (1991-05-01), Bailey et al.
patent: 5154862 (1992-10-01), Reagan et al.
Derwent Publications Ltd, London, GB; AN 77-88734Y & JP-A-52 129 627 (Tohoku University) 31 Oct. 1977.
Japan Abstracs of Japan, vol. 009313, No. JP 60147503 10 Dec. 1985 (Mitsui Kosen KK).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing a hollow silicon carbide fiber reinforce does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing a hollow silicon carbide fiber reinforce, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing a hollow silicon carbide fiber reinforce will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-746246

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.