ABSTRACT:
A method of manufacturing a dielectric from ferroelectric ceramic material having a perovskite structure with the basic formula ABO.sub.3. In the method, the dielectric is sintered in a reducing atmosphere and the sintered body is aftertreated at a temperature in the range of from 500.degree. to 900.degree. C. in an N.sub.2 --O.sub.2 atmosphere. The atmosphere contains a quantity of O.sub.2 corresponding to a partial O.sub.2 -pressure between 10.sup.-5 bar and 0.2 bar.

REFERENCES:
patent: 3920781 (1975-11-01), Eror et al.
patent: 4131444 (1978-12-01), Walker

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing a dielectric does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing a dielectric, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing a dielectric will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1944809

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.