ABSTRACT:
Method of manufacturing steel components containing 12 to 14% by weight of manganese having an austenitic structure, said parts being provided with steel end pieces having a mainly austenitic structure permitting their junction by welding to components made of any desired alloy, wherein, before applying thermal treatment, said end pieces are cast into moulds disposed directly at the ends of said manganese steel components. The ends of the manganese steel component are shaped and the end pieces are subsequently cast thereon in such a manner that each end of the part comprises a front surface inclined about a transverse horizontal axis.

REFERENCES:
patent: 1671412 (1928-05-01), Deppeler
patent: 1671413 (1928-05-01), Dickson
patent: 2633302 (1948-11-01), Cooper
patent: 3113359 (1963-12-01), Burke

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing 12 to 14% Mn steel components with welda does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing 12 to 14% Mn steel components with welda, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing 12 to 14% Mn steel components with welda will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-878117

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.