Method of making wear-resistant cylinder, or cylinder liner surf

Metal treatment – Process of modifying or maintaining internal physical... – Chemical-heat removing or burning of metal

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148 4, 148321, 148903, 148910, C21D 106

Patent

active

046170707

ABSTRACT:
In order to prevent the formation of fissures or tears in the walls of cylinders of an internal combustion engine, hardening tracks (4) generated by a carbon dioxide laser, are placed parallel to each other at an angle of inclination (.alpha.) with respect to the axis (3) of the wall of the cylinder or cylinder liner, and spaced from each other by a distance (X) which is greater than twice the distance (k) between the maxima (9, 10) of tension resulting in the operation of the ICE from the edges of the hardening track, thereby satisfying the condition: X is greater than 2.times.k.

REFERENCES:
patent: 4093842 (1978-06-01), Scott
patent: 4304978 (1981-12-01), Saunders
patent: 4313771 (1982-02-01), Lorenzo et al.
patent: 4452647 (1984-06-01), Sailas

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making wear-resistant cylinder, or cylinder liner surf does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making wear-resistant cylinder, or cylinder liner surf, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making wear-resistant cylinder, or cylinder liner surf will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1338892

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.