ABSTRACT:
A ternary single crystal relaxor piezoelectric grown from a novel melt using the Vertical Bridgeman method. The ternary single crystals are characterized by a Curie temperature, Tc, of at least 150° C. and a rhombohedral to tetragonal phase transition temperature, Trt, of at least about 110° C. The ternary crystals further exhibit a piezoelectric coefficient, d33, in the range of at least about 1200-2000 pC/N.

REFERENCES:
patent: 5342475 (1994-08-01), Yoshida et al.
patent: 5804907 (1998-09-01), Park et al.
patent: 5859211 (1999-01-01), Kreuder et al.
patent: 5998910 (1999-12-01), Park et al.
patent: 6238481 (2001-05-01), Yamashita et al.
patent: 2006/0012270 (2006-01-01), Han
patent: 2006/0091353 (2006-05-01), Matsushita et al.
patent: 2007243200 (2007-09-01), None
Luo J et al., Advances in Manufacturing Relaxor Piezpelectric Single Crystals', Applications of Ferroelectrics, 2007, ISAF 2007, Sixteenth IEEE International Symposium on, IEEE, Pl, May 1, 2007, pp. 557-560, XP031167419, ISBN: 978-1-4244-1333-1.
Luo J et al., “Elastic, Piezoelectric and Dielectric Properties of PIN-PMN-PT Crystals Grown by Bridgman Method”, Ultrasonics Symposium, 2008, IUS 2008, IEEE, IEEE, Piscataway, NJ, USA, Nov. 2, 2008, pp. 261-264, XP031443375, ISBN: 978-1-4244-2428-3.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making ternary piezoelectric crystals does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making ternary piezoelectric crystals, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making ternary piezoelectric crystals will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2710394

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.