Method of making synthetic diamond film with reduced bowing

Plastic and nonmetallic article shaping or treating: processes – Direct application of electrical or wave energy to work – Producing or treating inorganic material – not as pigments,...

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

264 121, 264 81, 264483, B29C 1100, B28B 3500

Patent

active

055871240

ABSTRACT:
A method for depositing synthetic diamond includes the following steps: (a) providing a deposition chamber; (b) providing a deposition surface in the deposition chamber, the deposition surface having a concave contour; (c) directing a plasma toward the concave deposition surface, the plasma including hydrogen and a hydrocarbon, such that synthetic diamond is formed on the concave deposition surface; and (d) releasing the synthetic diamond from the concave deposition surface to obtain free standing diamond, wherein the released diamond generally flattens.

REFERENCES:
patent: 4471003 (1984-09-01), Cann
patent: 4487162 (1984-12-01), Cann
patent: 4707384 (1987-11-01), Schachner et al.
patent: 4900628 (1990-02-01), Ikegaya et al.
patent: 4987002 (1991-01-01), Sakamoto et al.
patent: 4988421 (1991-01-01), Drawl et al.
patent: 5006203 (1991-04-01), Purdes
patent: 5114745 (1992-05-01), Jones
patent: 5124179 (1992-06-01), Garg et al.
patent: 5139372 (1992-08-01), Tanabe et al.
patent: 5204144 (1993-04-01), Cann et al.
patent: 5260106 (1993-11-01), Kawarada et al.
patent: 5270077 (1993-12-01), Knemeyer et al.
patent: 5294381 (1994-03-01), Iguchi et al.
patent: 5310512 (1994-05-01), Bigelow
patent: 5314652 (1994-05-01), Simpson et al.
Abstract (Dialog) From Diamond Film Update of Jun. 16, 1994 -"CVD Diamond Film Without Stress Cracks" (1 sheet).

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making synthetic diamond film with reduced bowing does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making synthetic diamond film with reduced bowing, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making synthetic diamond film with reduced bowing will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1176909

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.