ABSTRACT:
A method and apparatus for heat-treating nickel base superalloy articles to provide different properties in different regions of the article. An initially fine grain microstructure is heated such that a portion of the article is held above the .gamma.' solvus temperature long enough to provide a coarse grain microstructure while the remainder of the article remains below the .gamma.' solvus temperature and retains the fine grain microstructure. The coarse grain microstructure provides a reduced rate of fatigue crack growth rate while the fine grain microstructure retains good tensile properties. The invention is particularly applicable to the fabrication of turbine disks for gas turbine engines.
REFERENCES:
patent: 4680160 (1987-07-01), Helmink
patent: 4685977 (1987-08-01), Chang
patent: 4728374 (1988-03-01), Larson et al.
patent: 4816084 (1989-03-01), Chang
patent: 4820356 (1989-04-01), Blackburn
patent: 4820358 (1989-04-01), Chang
patent: 4888064 (1989-12-01), Chang
patent: 4907947 (1990-03-01), Hoppin, III
patent: 5100484 (1992-03-01), Wukusick et al.
patent: 5143563 (1992-09-01), Krueger et al.
Roy Upendra
Sohl Charles E.
United Technologies Corporation
LandOfFree
Method of making superalloy turbine disks having graded coarse a does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making superalloy turbine disks having graded coarse a, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making superalloy turbine disks having graded coarse a will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-874194