ABSTRACT:
Provided is a method of manufacturing an optical fiber preform from which an optical fiber having the desired characteristics can easily be produced. The method comprises the steps of: (1) preparing an intermediate preform for manufacturing an optical fiber preform; (2) measuring a refractive index profile in a radial direction at each of a plurality of positions in the longitudinal direction of the intermediate preform; (3) demarcating the outer diameter shape of the intermediate preform based on the result of the step of measuring the refractive index profile so that an optical fiber preform can be manufactured such that an optical fiber having the desired characteristics may be produced from the optical fiber preform; (4) elongating the outer periphery of the intermediate preform so that the outer diameter shape may be formed as demarcated in the step of demarcating the outer diameter shape; and (5) drawing, so as to have a substantially constant outer diameter, the intermediate preform that has been subjected to the grinding step.

REFERENCES:
patent: 6522818 (2003-02-01), Aso et al.
patent: 6938443 (2005-09-01), Fabian
patent: 2002/0041746 (2002-04-01), Kato et al.
patent: 2002/0174689 (2002-11-01), Onishi et al.
patent: 2005/0126227 (2005-06-01), Collaro
patent: 2005/0163444 (2005-07-01), Miyabe et al.
patent: 2000-347228 (2000-12-01), None
patent: 2002-293563 (2002-10-01), None
patent: 2003-020239 (2003-01-01), None
patent: 2003-040636 (2003-02-01), None
patent: 2004-029441 (2004-01-01), None
Legrand et al., “Impact of the longitudinal variations of the chromatic dispersion of the gain of fiber parametric amplifiers”, Optical Society of America, 2003, pp. 261-263.
Mussot et al., “Zero-dispersion wavelength mapping of a highly nonlinear optical fibre-based parametric amplifier”, ECOC 2004 Proceedings—vol. 2, pp. 190-191.
Watanabe et al., “Interband Wavelength Conversion of 320 Gb/s (32×10 Gb/s) WDM Signal Using a Polarization-Insensitive Fiber Four-Wave Mixer”, ECOC '87, Sep. 20-24, 1998, Madrid, Spain, pp. 85, 87.
Mollenauer et al., “Method for facile and accurate measurement of optical fiber dispersion maps”, Optics Letters / vol. 21, No. 21 / Nov. 1, 1996, pp. 1724-1726.
Inoue “Four-Wave Mixing in an Optical Fiber in the Zero-Dispersion Wavelength Region”, Journal of Lightwave Technology, vol. 10, No. 11, Nov. 1992, pp. 1553-1561.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making optical fiber and optical fiber made by the... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making optical fiber and optical fiber made by the..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making optical fiber and optical fiber made by the... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-3915432

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.