ABSTRACT:
A method for converting a high magnetic retentivity, high magnetic conductivity aluminum, nickel, cobalt and iron alloy to a substantially magnetically non-retentive alloy comprises heating the alloy to a temperature in the range 1400.degree. - 1500.degree. F. for about 30 minutes and quenching the heated alloy in a room temperature liquid coolant.
REFERENCES:
patent: 1752490 (1930-04-01), Karcher
patent: 1968569 (1934-07-01), Ruder
patent: 2002696 (1935-05-01), Kelsall
patent: 2027994 (1936-01-01), Mishima
patent: 2980563 (1961-04-01), Pavlovic et al.
patent: 3574003 (1971-04-01), Nara et al.
patent: 3783041 (1974-01-01), Tokushima
Lyman, et al. (ed) Metals Handbook, vol. 2, (Heat-Treating), Metals Park, Ohio (ASM) 1964 p. 16.
Duff, A, et al.; Physics, Philadelphia, 1947 pp. 260-262.
Bozorth, R; Ferromagnetism, New York, 1951 pp. 6, 386, 387.
BioMagnetics International Inc.
Friedman Stuart J.
Satterfield Walter R.
LandOfFree
Method of making non-retentive Al-Ni-Co-Fe alloy does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making non-retentive Al-Ni-Co-Fe alloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making non-retentive Al-Ni-Co-Fe alloy will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-70337