Method of making lithium-vanadium-oxide active material

Chemistry of inorganic compounds – Oxygen or compound thereof – Metal containing

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

429218, C01G 3100, H01M 458, C01D 1502

Patent

active

055498809

ABSTRACT:
A method of making an electrode active material of the nominal general formula LiV.sub.y O.sub.z where y is greater than 0 and up to about 3 and z is greater than 0 and up to about 8, comprises a series of steps. In the first step, lithium hydroxide is dispersed in an alcohol of the general formula C.sub.n H.sub.2n+1 OH. The alcohol and the hydroxide are each in an amount sufficient to provide a lithium alkoxide of the general formula LiOC.sub.n H.sub.2n+1. Next, progressive amounts of an oxide of vanadium having the general formula V.sub.2 O.sub.5 (vanadium pentoxide) are added while stirring the mixture. The amount of vanadium pentoxide in the mixture is sufficient to provide about 3 moles of vanadium for each mole of lithium present in the alkoxide. Then, the mixture is heated to an elevated temperature for a time sufficient to change the color of the oxide of vanadium and provide a solid precipitate. The solid precipitate is separated from the mixture and dried to obtain a powder of an oxide of vanadium having the nominal general formula LiV.sub.y O.sub.z, 0<y.ltoreq.3 and 0<z.ltoreq.8.

REFERENCES:
patent: 3063795 (1962-11-01), Smith
patent: 3063796 (1962-11-01), Kelmers
patent: 3728442 (1973-04-01), Pakhomov et al.
patent: 4061711 (1977-12-01), Morgan et al.
patent: 4119707 (1978-10-01), Thome et al.
patent: 4543341 (1985-09-01), Barringer et al.
patent: 4636248 (1987-01-01), Ogata et al.
patent: 4830939 (1989-05-01), Lee et al.
patent: 4879190 (1989-11-01), Lundsgaard
patent: 4918035 (1990-04-01), Inoue et al.
patent: 4920093 (1990-04-01), Nonaka et al.
patent: 4990413 (1991-02-01), Lee et al.
patent: 5013620 (1991-05-01), Miyazaki et al.
patent: 5023071 (1991-06-01), Sherif
patent: 5037712 (1991-08-01), Shackle et al.
patent: 5229225 (1993-07-01), Shackle
patent: 5326545 (1994-07-01), Koksbang et al.
patent: 5334334 (1994-08-01), Koksbang

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making lithium-vanadium-oxide active material does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making lithium-vanadium-oxide active material, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making lithium-vanadium-oxide active material will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1054741

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.