Metal treatment – Compositions – Heat treating
Patent
1975-03-14
1976-02-03
Stallard, W.
Metal treatment
Compositions
Heat treating
148 123, 148134, 148142, C21D 602, C21D 946
Patent
active
039363244
ABSTRACT:
A steel being substantially made and adjusted within the range of 0.04 to 0.12% C, 0.50 to 2.00% Si, and 0.10 to 1.60% Mn, passed through ordinary hot and cold rolling processes, is subjected to a full continuous annealing process comprising the following steps:
REFERENCES:
patent: 3839095 (1974-10-01), Kubotera et al.
patent: 3857740 (1974-12-01), Gondo et al.
Araki Kenzi
Fukunaka Shiro
Uchida Kuniki
Nippon Kokan Kabushiki Kaisha
Stallard W.
LandOfFree
Method of making high strength cold reduced steel by a full cont does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making high strength cold reduced steel by a full cont, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making high strength cold reduced steel by a full cont will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-2121253