ABSTRACT:
A metal-to-glass-to-metal seal that includes a chemical bond between the ss and metal as well as a mechanical seal is obtained by using an oxide layer which joins the glass and metal. A glass tube or glass powder with a coefficient of expansion which approximates the metal's coefficient of expansion is fitted between a pin and sleeve combination. Parts are then heated in a controlled dry hydrogen atmosphere to create a bond between the metal and glass.

REFERENCES:
patent: 3326618 (1967-06-01), Casamo et al.
patent: 4198225 (1980-04-01), Patrick et al.
patent: 4292464 (1981-09-01), Vogt et al.
patent: 4352951 (1982-10-01), Kyle
patent: 4377404 (1983-03-01), Hoshikawa et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making glass-to-metal seal (header) does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making glass-to-metal seal (header), we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making glass-to-metal seal (header) will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2029736

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.