ABSTRACT:
A tubular, porous ceramic electrode structure (3) is made from the sintered admixture of doped lanthanum manganite and an additive containing cerium where a solid electrolyte (4), substantially surrounds the air electrode, and a porous outer fuel electrode (7) substantially surrounds the electrolyte, to form a fuel cell (1).
REFERENCES:
patent: 4395468 (1983-06-01), Isenberg
patent: 4562124 (1985-12-01), Ruka
patent: 4751152 (1988-06-01), Zymboly
patent: 5106706 (1992-04-01), Singh et al.
Kuo Lewis J. H.
Ruka Roswell J.
Vasilow Theodore R.
Cillo Daniel P.
Maples John S.
Westinghouse Electric Corporation
LandOfFree
Method of making an air electrode material having controlled sin does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making an air electrode material having controlled sin, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making an air electrode material having controlled sin will most certainly appreciate the feedback.
Profile ID: LFUS-PAI-O-28989