Method of making a porous ceramic protective layer on an electro

Coating processes – Electrical product produced – Metallic compound coating

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

4271264, 501105, 204429, B05D 512

Patent

active

053105753

ABSTRACT:
An electrochemical measurement sensor for determining the oxygen content in gases, in particular in exhaust gases from internal combustion engines, having a solid electrolyte of stabilized zirconium dioxide and/or other oxygen ion-conductive oxides and at least one electrode on the side of the solid electrolyte exposed to the gas which is to be measured, is proposed, the electrode or electrodes containing, if desired, a ceramic support structure, and the electrode or electrodes exposed to the gas, which is to be measured, being covered by a porous ceramic protective layer of an Al.sub.2 O.sub.3 and/or Mg spinel (MgO.Al.sub.2 O.sub.3) matrix with preferably metastable ZrO.sub.2 particles incorporated therein.
The use of an Al.sub.2 O.sub.3 ZrO.sub.2 mixed oxide, which is preferably obtained by coprecipitation or by combination of suspensions of separately precipitated components or by spray-calcination of a combined solution of salts of the components and which may, if desired, contain a stabilizer for the ZrO.sub.2, such as, for example, Y.sub.2 O.sub.3, for forming the protective layer makes it possible, surprisingly, to form a firmly adhering, sintering-on protective layer which has a relatively narrow pore size distribution and which allows the best possible gas access to the outer electrode of the measurement sensor. The use of the Al.sub.2 O.sub.3 /ZrO.sub.2 mixed-oxide powder also achieves very extensive balancing of the hitherto observed mismatch of mechanical stresses and layer strengths on the one hand and the desired porosity and sensor control position on the other hand.

REFERENCES:
patent: 3935089 (1976-01-01), Togawa et al.
patent: 4199425 (1980-04-01), Sinkevitch
patent: 4225634 (1980-09-01), Tanaka et al.
patent: 4265930 (1981-05-01), Shinohara et al.
patent: 4296148 (1981-10-01), Friese
patent: 4402820 (1983-09-01), Sano et al.
patent: 4537865 (1985-08-01), Okabe et al.
patent: 4584086 (1986-04-01), Hayakawa et al.
patent: 4642174 (1987-02-01), Shibata
patent: 4859307 (1989-08-01), Nishizawa et al.
patent: 4915814 (1990-04-01), Harada et al.

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making a porous ceramic protective layer on an electro does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making a porous ceramic protective layer on an electro, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making a porous ceramic protective layer on an electro will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-2411629

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.