ABSTRACT:
A high temperature capability, water soluble polyester resin solution is made by esterifying an admixture comprising: an organic, aliphatic dihydric alcohol, an organic, polycarboxylic acid containing major portions of aromatic tricarboxylic acid, an organic, aliphatic dicarboxylic acid, and tris (2 hydroxy alkyl) isocyanurate; and then adding an amount of organic solvent effective to provide a solution; wherein the esterification is continued until the acid value drops to between about 35 to about 45 and wherein the mole ratio of OH/COOH=1.1 to 2.0.

REFERENCES:
patent: 3780133 (1973-12-01), Kolyer et al.
patent: 3835121 (1974-09-01), Preston
patent: 3849382 (1974-11-01), Nakatsuji et al.
patent: 3936404 (1976-02-01), Ishizuka et al.
patent: 4117032 (1978-09-01), Kwiecinski

LandOfFree

Say what you really think

Search LandOfFree.com for the USA inventors and patents. Rate them and share your experience with other people.

Rating

Method of making a high temperature capability water soluble pol does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making a high temperature capability water soluble pol, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making a high temperature capability water soluble pol will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFUS-PAI-O-1709500

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.